MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Radici Renycle® Renycle S GF3002HR 3039BK Polyamide 6
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Partially recycled PA6 30% glass fiber reinforced injection molding grade. Heat stabilized, hydrolysis resistant. Black color. Post industrial grade with low environmental impact compared to top grade material. Suitable for parts requiring medium stiffness and improved mechanical resistance.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccDAM; ISO 1183
Water Absorption 1.6 %
@Thickness 2.00 mm
50% RH; ISO 62
Moisture Absorption 6.20 %
@Thickness 2.00 mm
Immersion; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPa5mm / min. Conditioned; ISO 527-2/1A
 148 MPa5mm / min. DAM; ISO 527-2/1A
Elongation at Break 2.7 %5mm / min. DAM; ISO 527-2/1A
 4.5 %5mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 7.30 GPa1mm / min. Conditioned; ISO 527-2/1A
 9650 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 235 MPa2mm / min. DAM; ISO 178
Flexural Modulus 9000 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 7.00 J/cm²Conditioned; ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²Conditioned; ISO 179/1e/A
 6.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1e/A
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °C10°C/min; ISO 11357-1/-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 100 °C
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6907 / 293412

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.