Semitron® ESd 420 PEI Polyetherimide electro static dissipative shapes exhibit high strength and stiffness, and excellent resistivity in the 10E6 to 10E9 ohms per square range. This grade in particular excels in high temperature environments, making it ideal for extreme structural applications in semiconductor and electronics markets. |
formerly Semitron® ESd 420- CM |