MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco FM Seamer Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Seamer Oil FM is a premium performance industrial lubricant designed specifically to be used in Angelus Sanitary Can Machine Company seaming equipment and other similar applications.

This product was developed in consultation with Angelus Sanitary Can Machine Company and key customers.

It contains a special biocide to prevent growth of molds when the product comes in contact with water. Chevron Seamer Oil FM provides performance well above that found in typical mineral oils often used in the food industry.

Applications

Chevron Seamer Oil FM is intended for use in food processing industries where incidental food contact may occur.

Chevron Seamer Oil FM is engineered to exceed the requirements of and is approved by Angelus Sanitary Can Machine Company for use in the 61H, 62H, 120L, 121L, 140S, and 180S seamers, where an ISO 150 oil is specified. Chevron Seamer Oil FM is intended to extend the machinery`s life to overhaul.

Chevron Seamer Oil FM is recommended for:

  • FMC Rotary Cookers and Sterilizers due to its excellent antiwear properties
  • circulating systems that require an ISO 150 viscosity due to its excellent low foam properties and oxidation stability.

Key Words: CPS Number: 250223; MSDS Number: 6765
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31 °
Viscosity Measurement 111Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 746 SUS
Saybolt Viscosity at 210°F 81.3 SUS
Kinematic Viscosity at 40°C (104°F) 143 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.4 cStASTM D445
Oxidative Stability >= 15000 hourHours to 2.0 mg KOH/g acid number; ASTM D943
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.560 mm
 
Thermal PropertiesOriginal ValueComments
Pour Point -9.00 °CASTM D97
Flash Point 284 °CASTM D92
 
Descriptive Properties
Rust Procedure A, Distilled WaterPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV111 / 74726

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.