MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ChevronTexaco TDH® Special Oil
Categories: Fluid; Lubricant

Material Notes: Texaco TDH Oil Special delivers value through:
  • Lower operating costs — By delivering or exceeding the performance of fluids supplied by equipment manufacturers, helps in avoiding the cost of generally more expensive fluids and thereby lowers overall operating costs.
  • Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions leading to increased equipment life.
  • Lower inventory cost — One fluid does the job of a full range of mobile hydraulic systems. Can replace multiple products and free up shelf space too!
  • Minimizing weather and storage concerns — Protects against rust and corrosion of highly finished precision parts when operating in humid conditions and during seasonal shutdown periods.
  • Reduced downtime — Good compatibility with seals, O-rings, and packing materials maintains their good condition and keeps leakage at a minimum.
  • Smoother operation— By eliminating brake "chatter" and transmission "slip" they assure quiet and efficient action of brakes and transmission.
  • More reliable operation — Formulation keeps metal parts clean and free of varnish and sludge deposits that could result in premature breakdown.

Texaco TDH Oil Special is a high quality, multifunctional fluid, specially formulated for use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other equipment employing a common fluid reservoir.

It is formulated with high quality base stocks, a viscosity index improver, oxidation and corrosion inhibitors, antiwear and film strength additives, an antifoaming agent, and a pour point depressant.

The distinctive blue color of Texaco TDH Oil Special allows for easy product identification and leak detection.

Texaco TDH Oil Special meets the needs of modern tractors for a combination lubricant. It performs many functions, such as lubrication of the transmission and final drive, and serves as a hydraulic fluid to operate power steering units, brakes, implements, and attachments.

Furthermore, Texaco TDH Oil Special eliminates brake "chatter" and excessive brake facing wear, assures smooth operation of clutch packs and wet brakes, provides excellent shifting action, provides superior rust and corrosion protection for vital parts, minimizes leakage because of good compatibility with seals, Orings, and packing materials. It prevents sludge and varnish formation, protects metal surfaces against scuffing and wear, and provides outstanding lubrication for spur, helical, and spiral bevel final drive gears.

Texaco TDH Oil Special is compatible with equipment manufacturers proprietary fluids and other fluids of this type.

Texaco TDH Oil Special is specifically formulated to meet John Deere J20C.

It is recommended for use:

  • As a multifunctional fluid in all types of farm tractors and equipment.
  • In any application which calls for the following OEM lubricant specifications:
    • AGCO — improved power fluid 821XL
    • John Deere — J20C
    • Ford New Holland — ESN-M2C134-D, FNHA-2-C-201
    • Massey Ferguson — M1135, M1141, M1143
    • White Farm Equipment — Q-1826
    • Case Corporation — JIC-143, JIC-145, MS 1206, MS 1207, MS 1209, MS 1210 (TCH)
    • Oliver — Type 55
    • Minneapolis-Moline Fluids
    • Caterpillar TO-2
    • Renk — Bus ATF 873, 874 A/B
    • Allison C4
    • Kubota UDT
    • International Harvester B6

    Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

    CPS Number: 221899; MSDS Number: 10802

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.9 °
Brookfield Viscosity 40000 cP
@Temperature -35.0 °C
Viscosity Measurement 145Viscosity Index
Saybolt Viscosity at 100°F 298 SUS
Saybolt Viscosity at 210°F 58.3 SUS
Kinematic Viscosity at 40°C (104°F) 58.4 cSt
Kinematic Viscosity at 100°C (212°F) 9.5 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -42.0 °C
Flash Point 235 °C
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA198 / 77077

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.