MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cosmic Plastics FARBOSET® 2460 All Colors Mineral Filled Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Mineral Filled

Material Notes: Cosmic FARBOSET 2460 is a mineral-filled epoxy molding compound featuring fast cure rates, excellent moldability and superior thermal shock and moisture resistance. This compound was especially formulated for improved resistance to moisture ingress along with a high glass transition temperature for optimum reliability performance. It is designed to encapsulate a wide range of devices including tantalum and ceramic capacitors, resistors, resistor networks and high performance coils.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 g/cc
Bulk Density 1.00 g/ccpowder
Density 2.14 g/ccMolded
Linear Mold Shrinkage 0.0040 in/in
Spiral Flow 79.0 cmEMMI 1-66A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8000 psi
Flexural Strength 13000 psi
Flexural Modulus 1.95e+6 psi
Compressive Strength 25000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+15 ohm-cm
Dielectric Constant 5.2
@Frequency 1e+6 Hz
 5.4
@Frequency 10000 Hz
 5.6
@Frequency 60.0 Hz
Dielectric Strength 350 V/mil
@Thickness 3.17 mm
Dissipation Factor 0.012
@Frequency 1e+6 Hz
 0.014
@Frequency 60.0 Hz
 0.018
@Frequency 10000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 µm/m-°CAlpha 1
Glass Transition Temp, Tg 165 °C
Flammability, UL94 V-0
@Thickness 6.35 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 145 - 180 °C
Cure Time 1.00 - 2.00 min
@Temperature 150 °C
 27.0 sec
@Temperature 150 °C
Hot Plate
Shelf Life 0.0670 Month
@Temperature 35.0 °C
2 days
 0.250 Month
@Temperature 25.0 °C
1 week
 12.0 Month
@Temperature 4.00 °C
 
Descriptive Properties
Molding Pressure200-1000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade
Sumitomo Bakelite North America E 3812M-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler

PCOSM028 / 190810

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.