MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a pigment dispersion aid in polypropylene fiber applications. As a paraffin wax modifier it improves blocking, scuff, and abrasion resistance.
    Key Attributes:
  • Improves blocking, scuff, and abrasion resistance in paraffin wax blends
  • Low molecular weight
  • Polypropylene (PP) homopolymer
  • Useful in color concentrates, toner compounds, and as a pigment dispersion aid
    Application/Uses:
  • Building and Construction
  • Hot Melt Adhesives
  • Packaging
  • Solvent borne Adhesives
  • Wax Modification

Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D5
Viscosity 250 - 950 cP542-111
Brookfield Viscosity 700 cP
@Temperature 190 °C
Molecular Weight 12000 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 277 °C
Ring & Ball Softening Point 163 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0542-130
 
Descriptive Properties
Penetration Hardness<1 dmmASTM D5, Needle under 100-g load for 5s @ 25 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow HDPE 17450N High Density Polyethylene
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer
Dow Elvax® 650Q Ethylene Vinyl Acetate
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer
Total PPH 3825 Polypropylene, Injection Molding Grade

PWESF8913 / 133458

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.