MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 8000 - 14000 cPAccelerator
 20000 - 50000 cPBase
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80
Shear Strength 100 psiOverlap, Isopropyl Alcohol Wipe surface prep, Neoprene/Steel
 120 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Neoprene/Steel
 140 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, SBR/Steel
 150 psiOverlap, Isopropyl Alcohol Wipe surface prep, SBR/Steel
 220 psiOverlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
 300 psiOverlap, Isopropyl Alcohol Wipe surface prep, ABS
 330 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic
 350 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, PVC
 400 psiOverlap, Isopropyl Alcohol Wipe surface prep, Polycarbonate
 450 psiOverlap, Isopropyl Alcohol Wipe surface prep, Polystyrene
 475 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene
 500 psiOverlap, Isopropyl Alcohol Wipe surface prep, PVC
 500 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polycarbonate
 575 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, ABS
 800 psiOverlap, Isopropyl Alcohol Wipe surface prep, FRP
 1000 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol Wipe surface prep, FRP
 1400 psiOverlap, Isopropyl Alcohol Wipe surface prep, Phenolic
 1400 psiOverlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Phenolic
 2000 psiOverlap, Galvanized Steel Okite degrease Hot dip
 2100 psiOverlap, Galvanized Steel Okite degrease Electrodeposited
 2800 psiOverlap, CRS MEK/abrade/MEK
 3200 psiOverlap, Aluminum Oakite degrease
 3500 psiOverlap, Aluminum MEK/abrade/MEK
 3500 psiOverlap, CRS Oakite degrease
 4000 psiOverlap, Copper MEK/abrade/MEK
 4000 psiOverlap, Brass CDA 260
 4000 psiOverlap, Stainless Steel MEK/abrade/MEK
 4200 psiOverlap, Brass Cartridge
 4500 psiOverlap, Aluminum Etched
 4500 psi
@Temperature 23.0 °C
Aluminum, Overlap
 4500 psi
@Temperature -55.0 °C
Aluminum, Overlap
 220 psi
@Temperature 121 °C,
Time 900 sec
Aluminum, Overlap
 700 psi
@Temperature 82.0 °C,
Time 900 sec
Aluminum, Overlap
 1000 psi
@Time 1800 sec
Aluminum, Overlap
 1400 psi
@Time 3600 sec
Aluminum, Overlap
 2500 psi
@Time 14400 sec
Aluminum, Overlap
Peel Strength 25.0 pli
 40.0 pliT-Peel, CRS MEK/abrade/MEK, 5-8 mil bondline
 50.0 pliT-Peel, CRS Oakite degreased, 5-8 mil bondline
 60.0 pliT-Peel, Etched Aluminum, 17-20 mil bondline
 3.00 - 5.00 pli
@Temperature 82.0 °C
Aluminum, T-Peel
 5.00 - 10.0 pli
@Temperature -55.0 °C
Aluminum, T-Peel
 60.0 pli
@Temperature 23.0 °C
Aluminum, T-Peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.40e+14 ohm-cmASTM D257
Dielectric Strength 1100 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 59.0 µm/m-°CBelow Tg
 159 µm/m-°CAbove Tg
Thermal Conductivity 1.25 BTU-in/hr-ft²-°F
@Temperature 45.0 °C
 
Descriptive Properties
AppearanceAmberAccelerator
 Opaque, off-white
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive

PMM34647 / 169394

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.