MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Crosspolimeri FRAGOM PR/303 UV Flame Retardant Halogen Free Polyolefine
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefin thermoplastic compounds.

FRAGOM PR/303 UV: thermoplastic compound for power sheathing cables. Excellent self extinguishing properties. Easy to color. Good processability and excellent extrusion stability. General purposes: sheathing process, compression/pipe extrusion. The material contain UV resistant additive AS/NZS 3808:2000 HFI 75-90TP, HFS 75-90-110 TP

Certify: TI6, TM7, VDE 0207 HM4(K=0,7), IEC 60092-359 SHF1

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccISO 178
Melt Flow 2.0 - 4.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 46ISO 868
Tensile Strength >= 9.00 MPaISO 527
 >= 9.81 MPa
@Temperature 70.0 °C,
Time 14400 sec
Ageing in oil, SAE 20; IEC 60811
 >= 11.7 MPa
@Temperature 110 °C,
Time 1.73e+6 sec
Heat Ageing; IEC 60811
Elongation at Break >= 170 %ISO 527
 >= 149.6 %
@Temperature 70.0 °C,
Time 14400 sec
Ageing in oil, SAE 20; IEC 60811
 >= 221 %
@Temperature 110 °C,
Time 1.73e+6 sec
Heat Ageing; IEC 60811
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 90.0 °C
@Time 14400 sec
40%, Penetration; IEC 60811
Oxygen Index 36 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 120 °C
Zone 2 130 °C
Zone 3 140 °C
Zone 4 155 °C
Die Temperature 170 °C
Head Temperature 160 °C
Dry Time 3.00 hour
@Temperature 80.0 °C
 6.00 hour
@Temperature 80.0 °C
 
Descriptive Properties
Cold Flex-40°CISO 458
Halogen Content< 0,2%IEC 60754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS091 / 294175

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.