MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Adstif HA 748L Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif HA748L is a high crystallinity polypropylene homopolymer with very good long term thermal stability, high stiffness, high HDT, good surface hardness, and good pigment dispersion.  Typical customer applications are parts of electric appliances such as rice cooker, microwave oven, electric kettle, as well as food containers, house wares and base resin of compounds.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D 792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength, Yield 39.0 MPaASTM D 638
Elongation at Yield 8.0 %ASTM D 638
Flexural Modulus 2000 MPaASTM D 790
Izod Impact, Notched 30.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CASTM D648
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 5144L Homopolymer Polypropylene
Borealis HD905CF Polypropylene Homopolymer for Cast Film
Borealis Daplen™ ED206HP TPO Compound
ExxonMobil PP1074KNE1 Polypropylene Homopolymer
Ineos H07B-01 Polypropylene Homopolymer

PEQT7021 / 218660

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.