MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes: KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber and the strength of engineering plastics. In additions, they offer very good thermal stability, chemical resistance and weather resistance. KEYFLEX resins can be widely accepted as the replacement of thermoset rubbers.

Characterization:

  • High impact strength
  • Low specific gravity
  • Excellent resistance to chemicals and weathering
  • Good electrical properties
  • Various hardness grades (soft, semi-soft, and hard)
  • Colorability
  • Recyclability

Applications:

    Automotive:

    • Exterior: Bumper, air spoiler, mud guard, trim, side molding
    • Interior: Head liner, instrument panel skin, glass sealing, door trim skin
    • Others: Air intake hose, air duct, lamp packing, weather stripping, handle gasket, boots dust

    Others: Hose, packing, phone foots, gasket, insulation sheet (water protection sheet etc.), racket grip, booster cable, pump cable

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85 - 91ASTM D2240
Tensile Strength at Break 3.90 MPaASTM D412
Tensile Stress at Strain 2.90 MPa
@Strain 100 %
ASTM D412
Elongation at Break 500 %ASTM D412
Izod Impact, Notched NB
@Temperature -40.0 °C
ASTM D256
Tear Strength 280 pliASTM D790
Compression Set 29 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395
 47 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -58.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 200 °CExtrusion cylinder temperature
 180 - 210 °CBlow molding cylinder temperature
Rear Barrel Temperature 190 - 210 °C
Middle Barrel Temperature 200 - 220 °C
Front Barrel Temperature 210 - 230 °C
Nozzle Temperature 210 - 230 °C
Die Temperature 200 °FExtrusion
 200 - 220 °FBlow molding
Mold Temperature 5.00 - 40.0 °CBlow molding
 30.0 - 60.0 °CInjection molding
Drying Temperature 70.0 - 80.0 °C
Dry Time 2 hourHot Blast
Injection Pressure 49.03 - 98.07 MPa
Screw Speed 20 - 100 rpm
 
Descriptive Properties
Ozone ResistanceNo CrackASTM D518

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Celanese SO.F.TER Sofpur® Elastomer Modified TPU 01 Foot Ware Compound
LyondellBasell Hifax™ TRA-3263EC/1 Thermoplastic Olefin Resin
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin

PLGCHEM123 / 50944

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.