MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL-A-46146 specification. It is non-corrosive, fast setting and flowable. It can be widely used for many applications, particularly in aerospace and electronics. MasterSil 709 bonds well to a wide variety of substrates. The rapidity of the cure depends on the thickness of the layer and the humidity; the thicker the layer the slower the cure. MasterSil 709 is serviceable over the broad temperature range of -75°F to +400°F. MasterSil 709 has a moderate viscosity with good flow properties that can also be used as a conformal coating for electronics. Its color is translucent.

Key Features

  • Meets MIL-A-46146
  • Fast, room temperature curing
  • Moderate viscosity with good flow properties
  • Non-corrosive

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Viscosity 30000 - 40000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25 - 35
Tensile Strength at Break 400 - 500 psi
Elongation at Break 300 - 400 %
Shear Strength 100 - 200 psiTensile, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 2.5
@Frequency 60 Hz,
Temperature 25.0 °C
Dielectric Strength 500 V/mil
@Thickness 3.17 mm
Dissipation Factor 0.0010
@Frequency 60 Hz,
Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -75.0 °F
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 0.250 - 0.333 hour
Shelf Life 6.00 Month
@Temperature 23.9 °C
in original unopened containers
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Master Bond Mastersil 771 One Component, Non-Corrosive Silicone Adhesive
Master Bond FL901AO One Component Thermally Conductive Epoxy Adhesive Film
Master Bond FL901S One Component, Silver Filled Epoxy

PMASTB341 / 149588

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.