MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm ISOBLOC® H13 Hot Work Tool Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Hot Work Steel

Material Notes:

This premium H13 grade is an electroslag (ESR) steel, giving it excellent toughness making it suitable for demanding hot-work applications.

A premium grade H13 hot work tool steel featuring:

  • Very good toughness properties meeting the requirements of NADCA 207-97
  • Very good heat checking resistance
  • Good temper resistance and high temperature strength
  • Excellent polishability and texturability

Key Words: DIN 1.2344; JIS SKD61; 40CrMoV5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.282 lb/in³
 0.275 lb/in³
@Temperature 593 °C
 0.276 lb/in³
@Temperature 499 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 531870°F, 30 min Soak
 541920°F, 15 min Soak
Tensile Strength, Ultimate 52000 psi
@Temperature 649 °C
treated to 175 ksi)
 85000 psi
@Temperature 649 °C
treated to 230 ksi)
 160000 psi
@Temperature 316 °C
treated to 175 ksi)
 200000 psi
@Temperature 316 °C
treated to 230 ksi)
Tensile Strength, Yield 48000 psi
@Strain 0.2 %,
Temperature 649 °C
Heat treated to 175 ksi
 60000 psi
@Strain 0.2 %,
Temperature 649 °C
Heat treated to 230 ksi
 130000 psi
@Strain 0.2 %,
Temperature 316 °C
Heat treated to 175 ksi
 170000 psi
@Strain 0.2 %,
Temperature 316 °C
Heat treated to 230 ksi
Reduction of Area 50 %
@Temperature 316 °C
Heat treated to 175 ksi
 50 %
@Temperature 316 °C
Heat treated to 230 ksi
 55 %
@Temperature 649 °C
Heat treated to 230 ksi
 90 %
@Temperature 649 °C
Heat treated to 175 ksi
Modulus of Elasticity 31200 ksi
 23900 ksi
@Temperature 593 °C
 25500 ksi
@Temperature 499 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000520 ohm-cm
 0.0000860 ohm-cm
@Temperature 499 °C
 0.0000960 ohm-cm
@Temperature 593 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.40 µin/in-°F
@Temperature 93.3 °C
 6.90 µin/in-°F
@Temperature 399 °C
 7.30 µin/in-°F
@Temperature 704 °C
Specific Heat Capacity 0.110 BTU/lb-°F
 0.131 BTU/lb-°F
@Temperature 499 °C
 0.141 BTU/lb-°F
@Temperature 593 °C
Thermal Conductivity 25.0 W/m-Khardened
 26.8 W/m-Kannealed
 27.7 W/m-K
@Temperature 399 °C
hardened
 30.4 W/m-K
@Temperature 704 °C
hardened
 31.0 W/m-K
@Temperature 399 °C
annealed
 33.4 W/m-K
@Temperature 704 °C
annealed
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.39 %
Chromium, Cr 5.2 %
Iron, Fe 90.56 %As Balance
Manganese, Mn 0.40 %
Molybdenum, Mo 1.4 %
Silicon, Si 1.1 %
Sulfur, S <= 0.0030 %
Vanadium, V 0.95 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm SUPERIOR® H13 Hot Work Tool Steel
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
AISI Type H13 Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel

NBUCOR10 / 15479

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.