MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kraton® D1160 B (SIS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified:
Kraton D1160 BT - supplied as a porous pellet dusted with talc

Region: South America, Europe, Asia Pacific, North America, and Japan

Uses: Kraton D1160 B is used in formulating adhesives, in particular hot melt pressure sensitive adhesives.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccISO 2781
Bulk Density 0.350 g/ccASTM D1895
Volatiles <= 0.30 %KM 04
Brookfield Viscosity 700 - 1100 cP25% Toluene Solution at 25°C; KM 06
Molecular Weight 168000 - 188000 g/molKM 01
Melt Flow 5.0 - 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Ash <= 0.50 %BT; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 48
@Time 30.0 sec
Measured on compression molded slabs; ISO 868
Tensile Strength 32.0 MPaMeasured on films cast from a toluene solution; ISO 37
Elongation at Break 1300 %Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00190 GPa
@Strain 300 %
film cast from poluene solution; ISO 37
 
Descriptive Properties
ContentNon-staining phenolic antioxidant>0.08%, KM 08
 Polystyrene17.4-20.5%, KM 03
 Total Extractables<1.0%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® D2122 DO (SBS) Compound
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer

PKRA9862 / 132761

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.