MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lushan OR-1 Halogen-Free Flame-Retardant Compatibilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Halogen-free flame retardant compatibilizer Lushan series for cables and wires are developed by several doctors and maters from Lushan’s R&D Center, and combined ten years’ modified polyolefin grafting theories and haloen-free flame-retardant compatibilizer research. Lushan halogen-free flame retardant Compatibilizer can be widely used in the non-halogen flame retardant of hydroxides of metals, phosphorus, and nitrogen and so on to fill in the composite wire and cable materials, to improve the compatibility between the matrix resins and flame-retardant compatibilizer interfaces, and accelerate the flame-retardant compatibilizer spreading, and thus, halogen-free flame retardant compatiblizer interfaces, and accelerate the flame-retardant compatibilizer could enhance mechanics and processing capability and performance of flame retardant of wires and cables materials.

Compatibilizer Usage:

  • Compatibilzer widely used in composite cable and wire filled with metal hydroxides, phosphorus and nitrogen, and so on to improve the compatibility between the matrix resins and flame retardant compatibilizer interfaces
  • Fulfilling RoHS-normative standards, and SGS Halogen-testing standards
  • High grafting rate and low gel content
  • Excellent processing performance

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Index of Compound 3.0 g/10 min
 
Descriptive Properties
AppearanceNatural color granule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lushan LR-1D Halogen-Free Flame-Retardant Compatibilizer

PLUSH051 / 150049

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.