MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Expandable Polystyrene (EPS) R625B Expandable Polystyrene Resin  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Regular Grade with 25% Recycled Content

Features/Attributes:

  • 25% Recycled Content
  • Low Pentane
  • Fast Molding Cycles
  • Excellent Fusion/Part Strength
  • Recyclable in PS recycle steams

Applications:

  • General Purpose Packaging
  • Wine-Packs
  • Shippers/Coolers
  • Medical/Pharmaceutical Shippers

The thermal conductivity of expanded polystyrene at an average temperature of 75°F (24°C) 5s 36west at 3.5 pounds per cubic foot (pcf). It rises slightly at lower density until about 1.5 pcf where it increases rapidly. The rate of increase is much less at higher densities

  • 8.0 pcf (128 g/l) -- 0.269 Btu-in/(hr-ft2-°F) or 28.7 mW/(m-K)
  • 12.0 pcf (192 g/l) -- 0.276 Btu-in/(hr-ft2-°F) or 39.8 mW/(m-K)

R625 Resin with EcoSix™ recycled resin contains 25% of RAPA EcoSix™ resin, which is certified by Scientific Certification Systems to be 100% recycled content. NOVA Chemicals EPS resins are biologically and chemically inert. NOVA Chemicals EPS resins are do not contain CFC's (Chlorofluorocarbons).

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 38.0 - 40.0 lb/ft³
Density 0.0176 g/ccBatch Pre-Expander
Filler Content 4.2 %Pentane Content
 4.2 %Targeted Pentane Content
Particle Size 850 µm"B" Bead Size
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 30.0 psiat break
Compressive Strength 14.0 psi
@Strain 10 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µin/in-°F
Thermal Conductivity 0.210 - 0.240 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °F
 
Descriptive Properties
Pre-Puff Age Time (Hours)4-48Depending on pre-expanded density and method of bead pre-expansion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSI 3630 Medium Impact Polystyrene
Total Lacqrene® 2901 Medium Impact Polystyrene
Total Lacqrene® 2551 Medium Impact Polystyrene
SYNTHOS Koplen® 1020 FR Expandable Polystyrene
Sekisui PIOCELAN LSP-30EB Moldable Polymer Foam

PNOVB118 / 194726

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.