MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Ultramoll® IV HV Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Ultramoll® IV HV is a high viscosity polymeric plasticizer for a large number of polymers, e.g. polyvinyl chloride (PVC), VC copolymers, acrylonitrile-butadiene rubber (NBR), and polyurethane (PU). It is particularly suitable for the manufacture of foodstuff packaging.

Chemical composition: adipic acid polyester

General Ultramoll® IV HV as a plasticizer in polymer compounds shows:

  • good extraction resistance to oils and water
  • good migration resistance in contact with other polymers
  • good thermostability
  • good processability
Applications: Ultramoll® IV HV was specially developed for films based on polyvinyl chloride (PVC) for example cling films, which are expected to have good migration resistance in combination with a good processability. Ultramoll® IV is used in applications where foodstuff regulations and recommendations need to be met. Possible areas of applications are: Extrusion Oil and petrol-resistant film, hoses, cables and conveyor belts, conveyor belts for the foodstuffs industry, milking hoses, blown film (cling film and microwave film) for packaging foodstuffs. Injection moldingBoots, shoes and soles for applications requiring petrol and oil resistance, safety shoes, film for the automotive, packaging and office article industry Coatings industry Oil-resistant protective clothing for industrial use, oil and petrol-resistant tarpaulins

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.101 g/cc
@Temperature 60.0 °C
DIN 51 757
 1.108 g/cc
@Temperature 50.0 °C
DIN 51 757
 1.134 g/cc
@Temperature 23.0 °C
DIN 51 757
Water Absorption <= 0.10 %DIN 51 777
Viscosity 1000 cP
@Temperature 60.0 °C
DIN 53 015
 1600 cP
@Temperature 50.0 °C
DIN 53 015
 11000 cP
@Temperature 23.0 °C
DIN 53 015
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0[mg KOH/g]; DIN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Pour Point 8.60 °FISO 3016
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.467DIN EN ISO 6320
Gardner Color Number <= 6.0DIN ISO 6161
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearancealmost colorless, highly viscous liquid
Specifications179°CDissolution temp, DIN 53 408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Ultramoll® V HV Plastic Additive

PLANY9087 / 209478

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.