MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay Chemicals NOCOLOK® Thickener (water soluble)
Categories: Fluid

Material Notes: NOCOLOK® Thickener can be used in mixture with NOCOLOK® Binder, water and NOCOLOK® Flux to improve adhesion of the flux coating.

CAS-No.: 111-76-2

Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appliances

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/cc
Solids Content 13 - 17 %
Vapor Pressure 0.0987 atmbibliographical ref.
 
Thermal PropertiesOriginal ValueComments
Boiling Point 100 °Cbibliographical ref.
 
Descriptive Properties
Composition38-42%Solvent organic
Explosion limit0.011Lower
 0.106Higher
Solid volume16 l/100 kg
Viscosity15 s 4 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Chemicals NOCOLOK® Precoating (water soluble)
Solvay Chemicals NOCOLOK® Binder (water-based)
Sylvin Technologies 8960-60 Natural PVC Extrusion Compound
Sandvik DH45 Cemented Carbide for Woodworking
Novatec Novablend® 5021 PVC

WSOLV040 / 147689

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.