MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beryllium-Copper Alloy 50C, UNS C81800, TF00 Temper
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, Permanent Mold, Plaster, and Sand.

Applications: Resistance welding electrodes, dies

Test specimen: TF00 temper, aged 3 hours at 480°C, solution treated at 900-950°C.

Inactive per the Copper Development Association.

Key Words: BeCu; beryllium copper alloy 50C, CA 818, RWMA Class III
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.62 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 96
Tensile Strength, Ultimate 705 MPa
Tensile Strength, Yield 515 MPa
@Strain 0.2 %
Elongation at Break 8.0 %In 50 mm
Modulus of Elasticity 110 GPa
Poissons Ratio 0.33
Machinability 40 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 41.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000359 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 218 W/m-K
@Temperature 20.0 °C
Melting Point 1010 - 1070 °C
Solidus 1010 °C
Liquidus 1070 °C
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Solution Temperature 900 - 925 °C
Aging Temperature 480 °C
Casting Temperature 1120 - 1175 °CHeavy castings
 1175 - 1230 °CLight castings
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.10 %
Beryllium, Be 0.30 - 0.55 %
Chromium, Cr <= 0.10 %
Cobalt, Co 1.4 - 1.7 %
Copper, Cu >= 95.6 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.0020 %
Nickel, Ni <= 0.20 %
Silicon, Si <= 0.15 %
Silver, Ag 0.080 - 0.12 %
Tin, Sn <= 0.10 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium-Copper Alloy 50C, UNS C81800, As-cast
UNS C81100, Copper Casting Alloy
Beryllium Copper Alloy 10C, UNS C82000 TB00 Temper
Beryllium Copper, UNS C17000
Beryllium-Copper Alloy 30C, UNS C82200, TB00 Temper

MC81800b5 / 11865

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.