MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound DX13354X Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DX13354X compound is based on Polycarbonate (PC) resin containing 30% glass fiber. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Improved Impact, Good Surface Aesthetics, Wide Processing Window and Colorable.

Features: Aesthetics and Appearance,Enhanced Ductility,Laser Direct Structuring,Circuit Solution,Colorable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Density 1.43 g/ccISO 1183
Viscosity 13 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 280 °C
ASTM D1238
 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPa5 mm/min; ASTM D638
 90.0 MPa5 mm/min; ISO 527
Elongation at Break 2.1 %5 mm/min; ISO 527
 2.2 %5 mm/min; ASTM D638
Tensile Modulus 6600 MPa1 mm/min; ISO 527
 6900 MPa5 mm/min; ASTM D638
Flexural Strength 130 MPa1.3 mm/min, 50 mm span; ASTM D790
 130 MPa2 mm/min; ISO 178
Flexural Modulus 6300 MPa1.3 mm/min, 50 mm span; ASTM D790
 6400 MPa2 mm/min; ISO 178
Izod Impact Notched 90.0 JASTM D256
Izod Impact, Unnotched 500 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 36.0 kJ/m²ISO 179/2C
Charpy Impact, Notched 9.00 kJ/m²ISO 179/2C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.45
@Frequency 1.90e+9 Hz
SABIC method
 3.45
@Frequency 5.00e+9 Hz
SABIC method
 3.47
@Frequency 1.10e+9 Hz
SABIC method
Dissipation Factor 0.011
@Frequency 5.00e+9 Hz
SABIC method
 0.012
@Frequency 1.90e+9 Hz
SABIC method
 0.013
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 22.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 61.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 126 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 124 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 120 °C
@Thickness 3.20 mm
ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 295 °C
Zone 2 270 - 295 °C
Zone 3 270 - 295 °C
Melt Temperature 270 - 295 °CInjection Molding
Mold Temperature 100 - 120 °C
Drying Temperature 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81565 / 289512

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.