MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics MF120F Alumina Silicate
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Tailorable hardness with excellent high temperature capabilities. Can be formed to complex shapes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.30 g/ccFired
Porosity 2.0 - 3.0 %Apparent, can be made water resistant
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 50 - 95tailorable
Modulus of Elasticity 55.4 GPa
@Temperature 20.0 °C
Flexural Strength 64.0 MPa
@Temperature 20.0 °C
3-point
Compressive Strength 275 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 350000 ohm-cm
@Temperature 675 °C
 >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
Dielectric Constant 5.3
@Frequency 1e+6 Hz
Dielectric Strength 3.90 kV/mm
@Temperature 20.0 °C
dc
Dissipation Factor 0.010
@Frequency 1e+6 Hz
Dielectric Loss Index 0.036
@Frequency 1e+8 Hz
K*tan delta
 0.053
@Frequency 1e+6 Hz
K*tan delta
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.90 µm/m-°C
@Temperature 20.0 °C
 3.20 µm/m-°C
@Temperature 800 °C
Thermal Conductivity 1.26 W/m-K
@Temperature 300 °C
Maximum Service Temperature, Air 1150 °C
 
Descriptive Properties
Te Value595°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate
American Elements Titanium Nitride Nanoparticles
BYK Laponite® S485 Magnesium Aluminum Silicate
Morgan Advanced Ceramics AL 600™ Mac-A960W Aluminum Oxide Ceramic
Morgan Advanced Ceramics M120F Mac-AS970W Aluminum silicate Ceramic

CMORG39 / 90417

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.