MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M 7225 HP Indigo Optimized Polyester Label Product
Categories: Polymer; Adhesive

Material Notes: 3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1400, which is a high performance tackified acrylic designed for use in demanding environments. These products are optimized for use in the HP Indigo printing press. All products are pattern coated with a dry edge (no adhesive) to minimize adhesive ooze and press clean-up.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.900 milAdhesive
 2.00 milFacestock
 3.10 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.20 pli180° Peel, 12"/min., 1" wide sample; TLMI Method
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -29.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= -12.0 °CApplication
 <= 49.0 °CApplication
Shelf Life 12.0 Month
 
Descriptive Properties
Adhesive TypeP1400 Perm
Liner50# SC Remoist

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M SJ5000 Protective Product, Molded Shapes
3M Scotchkote™ CR 511 Epoxy Ceramic Surface
3M Scotchcal™ ElectroCut™ 404 Graphic Film
3M OFL010N Outdoor UL Recognized Lexan Label Products
3M FS022 Clear Polystyrene Label Products

PMM33439 / 168186

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.