MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Radici RADIPOL® 40AM130KH Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: N° CAS. 32131-17-2

Description: Polyamide 66, Low viscosity, 1,3% Titanium Dioxide, Heat stabilized

Typical Applications: Base polymer for melt spinning POY, FOY, LOY

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO1183
Viscosity 50000 cP
@Shear Rate 3000 1/s,
Temperature 290 °C
Apparent shear
 60000 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
Apparent shear
 70000 cP
@Shear Rate 60.0 1/s,
Temperature 290 °C
Apparent shear
Viscosity Measurement 2.46Relative, Solvent: sulphuric acid 95.7%; Polyamide concentration:0.01 g/ml
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CScanning rate 10°C/min; ISO 11357-1-3
 
Optical PropertiesOriginal ValueComments
Yellow Index <= 4.0 %
 
Descriptive Properties
Amino End Group52 meq/kgMA0014
Carboxylic end group73 meq/kgMA0014
Chip Size2.0x2.5x3.0 mm
ColorFull Dull
Granulometry1.7 g/100 chips
TiO2 content0.013MA0015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADICI031 / 313532

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.