MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Conventus Polymers DURAMIDE PA66LGF50 Nylon 66, 50% long glass fiber filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: DURAMIDE PA66LGF50 is a 50% long glass fiber filled Polyamide 66. It is made via Pultrusion method. It is available in natural, black, and colors. It is available in AMR, EUR, and APAC.

Information provided by Conventus Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 265 MPaASTM D638
Elongation at Break 1.5 - 2.0 %ASTM D638
Flexural Strength 372 MPaASTM D790
Flexural Modulus 2.375e+6 psiASTM D790
Izod Impact, Notched 8.20 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 488 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 560 - 590 °F
Rear Barrel Temperature 540 - 570 °F
Middle Barrel Temperature 550 - 580 °F
Front Barrel Temperature 560 - 590 °F
Nozzle Temperature 550 - 580 °F
Mold Temperature 200 °F
Drying Temperature 185 °F
Dry Time 4.00 hour
Moisture Content 0.18 %
Back Pressure 25.0 - 50.0 psi
Cushion 0.250 in
Screw Speed 30 - 50 rpm
 
Descriptive Properties
Suggested Max Regrind5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCONV812 / 248386

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.