MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Admex™ 525 Polymeric Plasticizer
Categories: Other Engineering Material

Material Notes: Product Description: Admex™ 525 is a low molecular weight, polymeric plasticizer. It is characterized by a mild ester odor and light color. It possesses low viscosity with a desirable ratio of cost/permanence.

Application/Uses:

  • Coatings
  • Decals/Graphics/Graphic Arts
  • Fabric/Furniture upholstery
  • Flexible PVC
  • PVAc water based adhesives

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Viscosity 50 cP
@Temperature 75.0 °C
 235 - 425 cP
@Temperature 25.0 °C
Vapor Pressure <= 0.00000128 atm
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 3.0
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 218 °C
Pour Point -9.00 °C
Flash Point 155 °CSetaflash Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5013 / 222207

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.