Moplen EP240P is a heterophasic copolymer with medium flow in injection molding. This grade is nucleated and characterized by a low temperature impact resistance. Moplen EP240P is typically used in crates, house wares and opaque containers. Applications: Crates, House wares, Opaque Containers, Sports, Leisure & ToysInformation provided by LyondellBasell. |