MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M4110  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade; PVC, Transparent

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 63.5 cmRelative Spiral Flow; 23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ASTM D2240
Tensile Strength, Yield 53.1 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 30 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2830 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 86.2 MPaASTM D790
Flexural Modulus 2830 MPaASTM D790
Izod Impact, Notched 53.4 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Injection Molded; ASTM D256A
 320 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 72.8 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 71.1 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
All colors; UL 94
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %
@Thickness 3.18 mm
ASTM D1003
Transmission, Visible 80 %
@Thickness 3.18 mm
CIE Illuminant C; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 204 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Contact, Unspecified Rating
 
Descriptive Properties
Agency RatingsNSF 14
 NSF 61
 NSF Unspecified Rating
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
 General Purpose
 Medium Flow
 Medium Impact Resistance
FormsPellets
PVC Cell Classification14454ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFluid Handling
 General Purpose

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Nakan® RMA 705 N PVC, Rigid Injection Molding Grade
Arkema Nakan® RMS 501 L PVC, Rigid Injection Molding Grade
Teknor Apex Sinvicomp SRF 3703 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid

PH1PN8843 / 102679

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.