MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wellman EcoLon® GF3012-BK1 Nylon 66, 25% Glass
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Post-Consumer Recycled (PCR).

Potential EcoLon® Applications: Engine cooling fan, Air intake manifolds, Exterior mirror back plate, Engine cooling shrouds, Low gloss black mirror Housing, Switch sockets, Wheel trim covers, Air cleaner cover, Blower wheels, Interior ashtray, NVH engine covers, Cam covers, Fastening parts, Cam cover baffle, Steering column switch, Air intake manifold, Sun visor base plate, Carrier gasket, Headlamp fasters, Door handles interior, Corrugated tube clip, Fascia brackets, Radiator end tank drain cock, Door handles exterior (painted), Radiator support bracket, Door handles exterior, Accelerator Pedals, Radiator end tank, HVAC valve door, Front end carrier, Ball bearing cages, Fuel pipe assembly, Oil level indicator, Air cleaner tray, Timing chain cover, Door window guides, Vent window handles, A/C evaporator filter retainers, Sleeve- trans. control selector, Housing- trans. Control selector, Carbon canisters, Carbon canister brackets.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183
Filler Content 25 %Glass; ISO 3451
Linear Mold Shrinkage, Flow 0.0050 cm/cmDIS 294
Linear Mold Shrinkage, Transverse 0.010 cm/cmDIS 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130 MPaISO 527
Elongation at Break 3.0 %ISO 527
Flexural Strength 190 MPaISO 178
Flexural Modulus 7120 MPaISO 178
Charpy Impact, Notched 8.00 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 235 °CISO 75
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 266 - 293 °C
Middle Barrel Temperature 260 - 293 °C
Front Barrel Temperature 260 - 293 °C
Nozzle Temperature 254 - 293 °C
Melt Temperature 271 - 293 °C
Mold Temperature 71.0 - 93.0 °C
Injection Pressure 34.0 - 138 MPa
Back Pressure 0.340 - 1.03 MPa
Screw Speed 30 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEL00819 / 249943

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.