System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Markforged 3D Printed H13 Tool Steel, Heat Treated
Categories:
Metal
;
3D Printing/Additive Manufacturing Metal
;
Ferrous Metal
;
Tool Steel
;
Hot Work Steel
Material Notes:
H13 tool steel is used for high temperature and wear applications such as molds and die casts, wear inserts and tooling, and forming punches and dies.
Information provided by Markforged, Inc.
Key Words:
Additive Manufacturing
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.45
g/cc
Porosity
<= 5.5 %
Mechanical Properties
Original Value
Comments
Hardness, Rockwell C
45
ASTM E8
Tensile Strength, Ultimate
1500
MPa
ASTM E8
Tensile Strength, Yield
1250
MPa
@Strain 0.2 %
ASTM E8
Elongation at Break
5.0 %
ASTM E8
Component Elements Properties
Original Value
Comments
Carbon, C
0.3 - 0.45 %
Chromium, Cr
4.7 - 5.5 %
Iron, Fe
89.5 - 91.9 %
As Balance
Manganese, Mn
0.2 - 0.5 %
Molybdenum, Mo
1.3 - 1.7 %
Phosphorus, P
<= 0.03 %
Silicon, Si
0.8 - 1.2 %
Sulfur, S
<= 0.03 %
Vanadium, V
0.8 - 1.2 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
Markforged 3D Printed H13 Tool Steel, As-Sintered
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 450°C
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
Crucible Steel 161 Tool Steel, High Carbon H13
NMARKF994 / 232705
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.