MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Ultrafelt Paper Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Ultrafelt Paper is a completely inorganic paper made from ceramic fibre which has mechanical strength comparable with that of most conventional ceramic fibre papers and which retains its strength to high temperature. The long fibres, a low shot content and a special needling operation form a strong product, easy to handle. Ultrafelt Paper can be used at temperatures of up to 1100°C with minimal loss in strength. It is recommended for applications that require a binder free product which has a good high temperature strength. Ultrafelt Paper has good chemical stability with resistance to most chemicals. Exceptions include phosphoric and hydrofluoric acids and strong alkalies. There is no water of combination and an extremely low boron content.

Applications:

  • Heat treatment: separator between the material being treated and its support
  • Heat shields
  • Parting agent between parts and conveyor belt for brazing furnace operations
  • Glass sagger mould linings
  • Die cut shapes for household appliances
  • Heat distributions and diffusion and mechanical cushioning in aircraft honeycomb brazing
  • Fire protection

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0960 g/cc
 0.128 g/cc
 0.160 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0500 W/m-K
@Temperature 200 °C
at 160kg/m3, 2.5mm thick
 0.0900 W/m-K
@Temperature 400 °C
at 160kg/m3, 2.5mm thick
 0.130 W/m-K
@Temperature 600 °C
at 160kg/m3, 2.5mm thick
 0.180 W/m-K
@Temperature 800 °C
at 160kg/m3, 2.5mm thick
 0.240 W/m-K
@Temperature 1000 °C
at 160kg/m3, 2.5mm thick
 
Component Elements PropertiesOriginal ValueComments
Al2O3 47 %
SiO2 53 %
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool 80 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 3000 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

CMORF7095 / 203393

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.