MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Perkadox AIBN Pharmaceuticals row 2,2'-Azodi(isobutyronitrile)
Categories: Other Engineering Material

Material Notes: 2,2’-Azodi(isobutyronitrile) (Perkadox AIBN) is the (azo)initiator most commonly employed in radical reactions, especially those using tri-n-butyltin hydride. At temperatures above about 60°C, Perkadox AIBN decomposes with evolution of nitrogen to generate isobutyronitrile radicals. Major examples of reactions are cyclizations and halogenation.

CAS number: 78-67-1

EINECS/ELINCS No.: 201-132-3

Applications: Perkadox AIBN can be successfully used for bulk, solution, suspension, polymerization of a wide variety of monomers, such as styrene, vinyl chloride, vinylidene, acrylonitrile, acrylates and methacrylates. Perkadox AIBN does not form oxygenated residues and does not cause oxidative degradation of pigmented of dyed polymer systems. For this reason, the color stability or transparent, dyed polymers, such as polymethylmethacrylate, is improved. 2,2’- Azodi(isobutyronitrile) (Perkadox AIBN) is also the (azo)initiator most commonly employed in radical reactions, especially those using tri-n-butyltin hydride.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.600 g/cc
Density 1.11 g/cc
Half-life 0.100
@Temperature 101 °C
[hr]
 1.00
@Temperature 82.0 °C
[hr]
 10.0
@Temperature 64.0 °C
[hr]
Molecular Weight 164.2 g/mol
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 104 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %
 
Descriptive Properties
AppearanceWhite crystalline solid
Assay= 98.0 %
Color= 20 Pt-Co13% solution in acetone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY779 / 286302

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.