MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sandvik 25.10.4.LB Covered electrodes
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 25.10.4.LB is a covered electrode with basic coating for welding of super duplex (austenitic ferritic) stainless steels like UNS S32750/32760 (e.g. Sandvik SAF 2507 and Zeron* 100). It gives a molybdenum alloyed super duplex weld metal and is designed for excellent positional welding, corrosion resistance and impact properties. The weld metal has especially good properties under severely corrosive conditions. Examples of properties are:
  • Excellent stress corrosion cracking resistance in chloride-containing media
  • Excellent pitting resistance
  • High resistance to general corrosion
  • High resistance to erosion corrosion and corrosion fatigue
Globular transfer gives a slightly convex bead with deeper penetration than rutile electrodes and cleaner weld deposits with less nonmetallic inclusions and impurities.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 298
Tensile Strength, Ultimate 913 MPa
Tensile Strength, Yield 765 MPa
@Strain 0.2 %
Elongation at Break 28 %
Charpy Impact 55.0 J
@Temperature -50.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.030 %
Chromium, Cr 25 %
Manganese, Mn 0.80 %
Molybdenum, Mo 4.0 %
Nickel, Ni 10 %
Nitrogen, N 0.25 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.60 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Type 254 SMO High-Nitrogen Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S31254
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-1
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
329 Stainless Steel, annealed pipe
302 Stainless Steel, 25% hardened strip

NSANDV5133 / 199697

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.