MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® A-361C with 15 MT Black Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Intermediate viscosity level (when compared with Viton® A-201C/Viton® A-401C)
  • Fully precompounded with reduced curative level and Incorporated metal adhesion promoter
  • Improved processing with increased mold flow, easier mold release with less mold fouling, and improved demolding “hot tear”
  • Good metal bonding with standard industrial primers

Applications

  • Compression, transfer, and injection molding of: O-rings and gaskets, Valve stem and crankshaft seals (and other bonded parts requiring fluid and heat resistance of the A-family of Viton®)

    Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 52
@Temperature 121 °C
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6524 hours Postcure; ASTM D2240
 66No Postcure; ASTM D2240
Tensile Strength at Break 8.60 MPaNo Postcure; ASTM D412
 10.4 MPa24 hours Postcure; ASTM D412
Elongation at Break 244 %24 hours Postcure; ASTM D412
 313 %No Postcure; ASTM D412
100% Modulus 0.00210 GPa
@Strain 100 %
No Postcure; ASTM D412
 0.00270 GPa
@Strain 100 %
24 hours Postcure; ASTM D412
Compression Set 9.0 %
@Temperature 23.0 °C,
Time 252000 sec
O-Rings; ASTM D395B
 15 %
@Temperature 200 °C,
Time 252000 sec
O-Rings; ASTM D395B
 35 %
@Temperature 232 °C,
Time 252000 sec
O-Rings; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 °C
@Time 601 sec
Slab Cure
 232 °C
@Time 86400 sec
Postcure
 
Descriptive Properties
Formulation as Tested100A361C
 15MT Black
 3MgO
 6Ca(OH)2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Chemours Viton® GF-600S with 3phr, 802-40KE Fluoroelastomer Compound
Chemours Viton® GBLT-600S with 10022 Fluoroelastomer Compound
Chemours Viton® GBLT-600S Fluoroelastomer Compound
Chemours Viton® GBL-200S Fluoroelastomer Compound

PDVC9904 / 170545

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.