System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LEXAN™ Copolymer EXL9112 Polycarbonate (PC) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA.
Features: High Impact Resistance
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.18
g/cc
ASTM D792
Density
1.19
g/cc
ISO 1183
Moisture Absorption
0.0200 %
Injection Molding
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
0.35 %
ISO 62-1
Viscosity
16
cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
17
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
95.0
MPa
H358/30; ISO 2039-1
Tensile Strength at Break
55.0
MPa
50 mm/min; ISO 527
58.0
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
58.0
MPa
50 mm/min; ASTM D638
59.0
MPa
50 mm/min; ISO 527
Elongation at Break
100 %
50 mm/min; ISO 527
103 %
50 mm/min; ASTM D638
Elongation at Yield
5.0 %
50 mm/min; ISO 527
5.8 %
50 mm/min; ASTM D638
Tensile Modulus
2200
MPa
1 mm/min; ISO 527
2260
MPa
50 mm/min; ASTM D638
Flexural Strength
88.0
MPa
yield, 2 mm/min; ISO 178
95.0
MPa
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2300
MPa
2 mm/min; ISO 178
2330
MPa
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
731
J
ASTM D256
560
J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO)
53.0
kJ/m²
80*10*4; ISO 180/1A
55.0
kJ/m²
80*10*3; ISO 180/1A
18.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
20.0
kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
80*10*3; ISO 180/1U
NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact, Notched
60.0
kJ/m²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
25.0
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
67.0
J
ASTM D3763
Electrical Properties
Original Value
Comments
Dielectric Constant
2.7
@Frequency 1e+6 Hz
IEC 60250
2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength
19.0
kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor
0.00040
@Frequency 50.0 - 60.0 Hz
IEC 60250
0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
175
V
IEC 60112
175
-
250
V
UL 746A
Hot Wire Ignition, HWI
15
-
30
sec
@Thickness >=0.800 mm
UL 746A
30
-
60
sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI
15
-
30
arcs
@Thickness >=0.800 mm
UL 746A
>=
120
arcs
@Thickness >=1.50 mm
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
72.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
75.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
72.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
75.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test
125
°C
PASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
136
°C
Edgew 120*10*4 sp=100mm; ISO 75/Be
136
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
124
°C
Edgew 120*10*4 sp=100mm; ISO 75/Ae
123
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
143
°C
Rate B/50; ASTM D1525
143
°C
Rate B/50; ISO 306
144
°C
Rate B/120; ISO 306
UL RTI, Electrical
130
°C
UL 746B
UL RTI, Mechanical with Impact
120
°C
UL 746B
UL RTI, Mechanical without Impact
130
°C
UL 746B
Flammability, UL94
HB
@Thickness >=0.800 mm
UL 94
V-0
@Thickness >=1.50 mm
UL 94
5VB
@Thickness >=2.50 mm
UL 94
5VA
@Thickness >=3.00 mm
UL 94
Oxygen Index
40 %
ISO 4589
Glow Wire Ignition Temperature
825
°C
@Thickness 1.00 mm
IEC 60695-2-13
825
°C
@Thickness 1.50 mm
IEC 60695-2-13
825
°C
@Thickness 2.00 mm
IEC 60695-2-13
825
°C
@Thickness 2.50 mm
IEC 60695-2-13
825
°C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
IEC 60695-2-12
960
°C
@Thickness 1.50 mm
IEC 60695-2-12
960
°C
@Thickness 2.00 mm
IEC 60695-2-12
960
°C
@Thickness 2.50 mm
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Nozzle Temperature
290
-
310
°C
Zone 2
280
-
305
°C
Zone 3
295
-
315
°C
Melt Temperature
295
-
315
°C
Injection Molding
Mold Temperature
70.0
-
95.0
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
48.0
hour
Cumulative; Injection Molding
Back Pressure
0.300
-
0.700
MPa
Shot Size
40 - 60 %
Vent Depth
0.00250
-
0.00760
cm
Screw Speed
40
-
70
rpm
Descriptive Properties
UV-light, water exposure/immersion
F1
UL 746C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80224 / 288171
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.