Ultra-clear material with high transparency. End products are biocompatible. Meet criteria regarding irritation, sensitization and cytotoxicity for biological assessment of medical products (DIN ISO 10993). Can be steam sterilized over longer period (>15 min.) Applications: Wide range of medical application such as surgical patterns or operation models Information provided by Genistar. |