MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ XCY630 PC+ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC/ABS, hydrolytically stable.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Density 1.14 g/ccISO 1183
Water Absorption 0.40 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Viscosity 170 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 22 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 26 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.0 MPa50 mm/min; ASTM D638
 53.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa50 mm/min; ISO 527
 54.0 MPa50 mm/min; ASTM D638
Elongation at Break 120 %50 mm/min; ASTM D638
 120 %50 mm/min; ISO 527
Elongation at Yield 4.5 %50 mm/min; ISO 527
 4.5 %50 mm/min; ASTM D638
Tensile Modulus 2250 MPa1mm/min; ISO 527
 2300 MPa5 mm/min; ASTM D638
Flexural Yield Strength 82.0 MPa2 mm/min; ISO 178
 89.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2200 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 590 J/mASTM D256
 430 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 65.0 kJ/m²80*10*3; ISO 180/1A
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 65.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 30.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 55.0 JASTM D3763
 67.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 126 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 105 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 107 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 126 °CRate B/50; ISO 306
 126 °CRate B/50; ASTM D1525
 127 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 240 - 280 °CInjection Molding
Zone 1 230 - 260 °C
Zone 2 250 - 290 °C
Zone 3 250 - 290 °C
Melt Temperature 260 - 290 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10778 / 244245

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.