Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber, 40% Filler by Weight Additive: Heat Stabilized and Molybdenum Disulfide Lubricant Features: Lubricated and Heat Stabilizer Appearance: Black Information provided by TP Composites, Inc. |