MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop.
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Glass Bead Filled; Polypropylene, Glass Reinforced, Impact Modified

Material Notes: Features

Modified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to the modification. Delivered in natural mode and in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Linear Mold Shrinkage 0.0226 cm/cm
Linear Mold Shrinkage, Transverse 0.021 cm/cm
Melt Flow 6.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPa
Elongation at Break 10 %
Tensile Modulus 1700 MPa
Flexural Strength 40.0 MPa
Flexural Modulus 1800 MPa
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature -20.0 °C
 35.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
 3.00 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °C
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
Vicat Softening Point 105 °CB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 40.0 - 80.0 °C
Injection Pressure 70.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Forging Brass, UNS C37700
Alliance N-35H Neodymium Iron Boron Magnetic Material
Chicago Extruded Metals UNS C37700 Copper-Zinc-Lead Alloy
Techmer ES HiFill® PP GB50 50% Glass Beads Filled
Techmer ES HiFill® PP GB40 40% Glass Beads Filled

PPLACO237 / 120861

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.