MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade; High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Production Method: Copolymerization of eythylene at low pressure pipes and connection elements for pipeline phase method.

Application: Composition is intended to be processed into pressure pipes and connection elements for pipeline systems, and high-strength thick films with thickness of 20 microns and higher.

Information Provided by Kazanorgsintez

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.947 - 0.950 g/cc
@Temperature 23.0 °C
 0.949 - 0.952 g/cc
@Temperature 20.0 °C
Volatiles <= 0.035 %
Melt Flow 5.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
±10%
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 20.0 MPa
Elongation at Break >= 600 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
@Time >=1200 sec
 
Descriptive Properties
Stability at Constant Internal Pressure 20°C; hr2500with initial wall stress 11.6 MPa
Stability at Constant Internal Pressure 80°C, initial wall stress 2.8 MPa, hr1000
Stability at Constant Internal Pressure 80°C; initial wall stress 4.0 MPa, hr165

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Formosa Plastics Formolene® HP4306 Pipe HDPE
LyondellBasell Hostalen CRP 100 W BLUE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 S YELLOW High Density Polyethylene (HDPE), Pipe Grade
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite

PKAZAN008 / 127327

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.