MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Zircar Ceramics AX-200 Refractory Supported Heater
Categories: Ceramic; Oxide; Metal

Material Notes: ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stable, high temperature refractory body.

AX-200 precision fabricated high temperature heaters will produce uniform, reliable heat to 1100ºC (2012ºF). They are 100% organic free and will not smoke or outgas when heated. 

Typical Applications:

  • Heating source in furnaces and industrial process equipment operating to 1100ºC (2012ºF).
  • High temperature hot plate heating element.
  • Molten metal splash resistant heating source for launders, troughs and distribution boxes.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00410 GPa
@Temperature 816 °C
Compressive Strength 27.6 MPa
@Temperature 816 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.860 W/m-K
@Temperature 538 °C
 0.900 W/m-K
@Temperature 1100 °C
Maximum Service Temperature, Air 1300 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 47 %
CaO 8.5 %
Other, total <= 4.5 %Including TiO2
SiO2 40 %
TiO2 <= 4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast L-40 Insulating Refractory
Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast 220HT Refractory Castable
Pyrotek Ceramite® CSR-S Refractory

CZIR904 / 138546

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.