MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik REWOQUAT® W 3690 PG Finishing Product
Categories: Fluid

Material Notes: Product description: 1-methyl-2-noroleyl-3-oleic acid amidoethyl imidazolinium methosulfate

Application: REWOQUAT® W 325 PG is recommended for the finishing of non-wovens, yarns, woven or knitted goods made of cotton or cotton blends, especially when good re-wetting properties are requested (terry cotton and knitted goods prepared for printing). REWOQUAT® W 3690 PG is a cationic hydrophilic softener. It is useful as a coupler and co-emul-sifier for cationic formulations. REWOQUAT® W 3690 PG can be used to formulate high concentrated dispersions.

Properties / Benefits: REWOQUAT® W 3690 PG contains no flammable solvent. REWOQUAT® W 3690 PG is an easy to handle, highly substantive liquid cationic surfactant with weak emulsifying properties. REWOQUAT® W 3690 PG is a substantive softener. It is dispersible in water and imparts excellent re-wetting properties to the treated fabrics. It is usable for the production of high concentrated aqueous dispersions. REWOQUAT® W 3690 PG is rather yellowing on white fabrics. It imparts ozone-fade resistance to the treated fabrics or garments (jeans).

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 4.0 - 5.55% in IPA/water
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 7.0
 
Descriptive Properties
Appearanceyellow, clear liquid
Content74-77%Active matter, mw=723

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik REWOQUAT® W 3690-90
Evonik REWOQUAT® WE 15 DPG Finishing Product
Evonik REWOQUAT® W 325 PG Finishing Product

PEVONIL525 / 196729

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.