System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC VALOX™ 8032U PBT (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.58
g/cc
ASTM D792
Density
1.53
g/cc
ISO 1183
Water Absorption
0.16 %
23°C/sat; ISO 62
Moisture Absorption
0.0500 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0040
-
0.0080
cm/cm
SABIC method
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0060
-
0.010
cm/cm
SABIC method
0.0060
-
0.010
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
15
g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D1238
15
g/10 min
@Load 2.16 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
119
ISO 2039-2
Ball Indentation Hardness
110
MPa
ISO 2039-1
Tensile Strength at Break
115
MPa
5 mm/min; ASTM D638
145
MPa
5 mm/min; ISO 527
Tensile Strength, Yield
115
MPa
5 mm/min; ASTM D638
145
MPa
5 mm/min; ISO 527
Elongation at Break
2.0 %
5 mm/min; ASTM D638
2.5 %
5 mm/min; ISO 527
Elongation at Yield
2.0 %
5 mm/min; ASTM D638
2.4 %
5 mm/min; ISO 527
Tensile Modulus
9500
MPa
1mm/min; ISO 527
9950
MPa
5 mm/min; ASTM D638
Flexural Strength
210
MPa
2 mm/min; break; ISO 178
Flexural Yield Strength
165
MPa
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
8450
MPa
1.3 mm/min, 50 mm span; ASTM D790
8500
MPa
2 mm/min; ISO 178
Izod Impact, Notched
57.0
J/m
ASTM D256
48.0
J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched
480
J/m
ASTM D4812
470
J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO)
9.00
kJ/m²
80*10*4; ISO 180/1A
8.00
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
8.00
kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
45.0
kJ/m²
80*10*4; ISO 180/1U
40.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched
45.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
40.0
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
9.00
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
9.00
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
8.00
J
ASTM D3763
Taber Abrasion, mg/1000 Cycles
30
CS-17, 1 kg; SABIC method
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
ROA; IEC 60093
Dielectric Constant
3.2
@Frequency 1e+6 Hz
IEC 60250
3.3
@Frequency 50.0 - 60.0 Hz
IEC 60250
3.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength
15.0
kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
23.0
kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
27.0
kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor
0.00080
@Frequency 50.0 - 60.0 Hz
IEC 60250
0.013
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
300
V
IEC 60112
250
-
400
V
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
22.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
25.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow
75.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
81.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Hot Ball Pressure Test
125
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
217
°C
Edgew 120*10*4 sp=100mm; ISO 75/Be
208
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
195
°C
1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
190
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
202
°C
Rate B/50; ASTM D1525
202
°C
Rate B/50; ISO 306
204
°C
Rate B/120; ISO 306
220
°C
Rate A/50; ASTM D1525
220
°C
Rate A/50; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
UL 94 by SABIC-IP
Processing Properties
Original Value
Comments
Processing Temperature
40.0
-
60.0
°C
Hopper Temperature
Nozzle Temperature
265
-
275
°C
Injection Molding
Zone 1
240
-
260
°C
Zone 2
255
-
280
°C
Zone 3
260
-
280
°C
Melt Temperature
260
-
285
°C
Mold Temperature
60.0
-
110
°C
Drying Temperature
110
-
120
°C
Injection Molding
Dry Time
4.00
-
6.00
hour
Injection Molding
Moisture Content
0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10260 / 243727
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.