MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Henkel Loctite® 246 High Temperature/Medium Strength Threadlocker
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Threadlockers
Invented by Loctite Corporation to lock seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from delicate electronic components to heavy construction equipment.

Loctite® Pre-Applied Threadlockers are dry-to-the-touch films applied to threaded fasteners by fastener suppliers and process centers located throughout North America. Ideally suited for OEMs, they improve speed of assembly and ensure quality by eliminating on-line adhesive dispensing.

Loctite® Threadlockers are available in varying viscosities and strengths for virtually any application, including exposure to extreme environments.

Loctite® 246 High Temperature/Medium Strength Threadlocker
This threadlocker resists oil and mild surface contamination at continuous temperatures to 450ºF. Suitable for fasteners between 0.25" and 0.75" (6 to 20 mm) diameters.

Torque capability, M10 steel nuts and bolts: 170 in. lbs. (break), 48 in. lbs. (prevail). Recommended Primer: 7649(N) or 7471(T) Typical Use: High temperature, medium strength

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
Viscosity 2600 cP
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 min
 24.0 hour
@Temperature 25.0 °C
Full Cure; Steel
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 4799 Industrial Adhesive
Master Bond FLM36-LO Film Adhesive
Master Bond FLM36 B-staged film for high performance bonding and sealing
Master Bond FL901S One Component, Silver Filled Epoxy
Hexcel® Redux® HP655 Toughened BMI film Adhesive

PLOCT092 / 51828

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.