CYCOM® 7668 resin is a 350°F (177°C) curing flame retardant epoxy formulated for use with fiberglass in structural laminates and sandwich panels for aircraft exteriors. Woven fabric impregnated with 7668 resin will maintain good tack and drape for at least 15 days at 75°F (24°C) and once cured, exhibits excellent resistance to thermal aging. Features & Benefits: - Four tailored tack levels
- Excellent flammability
- Resistant to thermal aging
- Outstanding tension, compression and sandwich properties
- Suitable for laminates and sandwich panels
- Low flow and core movement
- Meets BMS-8-139 and MIL-R-9300, type 2
- 350°F (177°C) cure
- 350°F (177°C) dry service temperature
- Shelf life 270 days at 10°F (-12°C) or below
- Handling life 15 days at 75°F (24°C)
- Mechanical life 30 days at 75°F (24°C)
Applications: Structural laminates and honeycomb core sandwich panels for aircraft exteriorsInformation provided by Cytec, subsequently acquired by Solvay. |