MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik SANMAC 304/304L Bar Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Sandvik SANMAC 304/304L, 1.4301/1.4307, is an austenitic chromium-nickel steel with improved machinability.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 215
Tensile Strength, Ultimate 515 - 680 MPa
 >= 360 MPa
@Temperature 500 °C
 >= 380 MPa
@Temperature 300 °C
 >= 380 MPa
@Temperature 400 °C
 >= 400 MPa
@Temperature 200 °C
 >= 450 MPa
@Temperature 100 °C
Tensile Strength, Yield >= 205 MPa
@Strain 0.2 %
 >= 230 MPa
@Strain 1 %
 >= 92.0 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 98.0 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 110 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 120 MPa
@Strain 1 %,
Temperature 500 °C
 >= 125 MPa
@Strain 1 %,
Temperature 400 °C
 >= 127 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 135 MPa
@Strain 1 %,
Temperature 300 °C
 >= 155 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 155 MPa
@Strain 1 %,
Temperature 200 °C
 >= 190 MPa
@Strain 1 %,
Temperature 100 °C
Elongation at Break >= 45 %
Reduction of Area >= 50 %
Modulus of Elasticity 200 GPa
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 300 °C
 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
 17.0 µm/m-°C
@Temperature 30.0 - 200 °C
 17.5 µm/m-°C
@Temperature 30.0 - 300 °C
 18.0 µm/m-°C
@Temperature 30.0 - 400 °C
 18.5 µm/m-°C
@Temperature 30.0 - 600 °C
 18.5 µm/m-°C
@Temperature 30.0 - 500 °C
 19.0 µm/m-°C
@Temperature 30.0 - 700 °C
Specific Heat Capacity 0.475 J/g-°C
@Temperature 20.0 °C
 0.500 J/g-°C
@Temperature 100 °C
 0.530 J/g-°C
@Temperature 200 °C
 0.560 J/g-°C
@Temperature 300 °C
 0.580 J/g-°C
@Temperature 400 °C
 0.600 J/g-°C
@Temperature 500 °C
 0.615 J/g-°C
@Temperature 600 °C
 0.625 J/g-°C
@Temperature 700 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 16.0 W/m-K
@Temperature 100 °C
 18.0 W/m-K
@Temperature 200 °C
 20.0 W/m-K
@Temperature 300 °C
 22.0 W/m-K
@Temperature 400 °C
 23.0 W/m-K
@Temperature 500 °C
 25.0 W/m-K
@Temperature 600 °C
 26.0 W/m-K
@Temperature 700 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 18.5 %
Iron, Fe 70.8 %As Balance
Manganese, Mn 1.8 %
Nickel, Ni 8.5 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.30 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 304L Stainless Steel
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
Sandvik 303-6RA11 Billet
Sandvik SANMAC 304/304L Billet
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar

NSANDV142 / 19036

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.