LACQRENE® 4801 is an easy flowing, high impact polystyrene for injection molding. The very good processing characteristics of this grade allows for the production of thin articles with long flow paths or complex shapes. A high level of mechanical properties are retained at very low temperatures (-40°C) which makes this grade particularly suitable for ice cream containers. Applications: Ice cream containers, Models, Presentation boxes, General containers, Medical products Information provided provided by Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |