MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Indium Corp. IndiOx® In2O3 Type A Indium Oxide, Crystalline Powder
Categories: Ceramic; Oxide

Material Notes: Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used as a resistive element in integrated circuits and to form heterojunctions with p-InP, n-GaAs and other semiconductors. Other uses include glass coloring, in alkaline batteries to suppress gassing and as an anti-arcing additive in high current electrical switches and contactors.

When doped with tin dioxide, thin films of indium-tin oxide (ITO) function as a transparent electrical conductor and can reflect a portion of the infrared spectrum. The major use of indium oxide is in the manufacture of ITO sputtering targets for thin film coating.

Type A - Crystalline: The primary particles range from 0.4 to 1.0 microns in diameter; agglomerates up to approximately 30 microns.

Properties

  • Chemical Formula: In2O3
  • General Description: Bright yellow powder
  • Purity Grades Available: 4N (99.99%), 5N (99.999%)
  • Solubility: Insoluble in water and alcohol.

Uses

  • Manufacturing of ITO sputtering targets and evaporation charges
  • Coloring ceramics and glasses

Information provided by the manufacturer, Indium Corporation of America.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.20 g/cc
Particle Size 0.40 - 1.0 µmprimary particles
 1.7 - 10.3 µmd10 agglomerates
 6.0 - 23 µmd50 agglomerates
 14 - 38 µmd90 agglomerates
Specific Surface Area 0.424 m²/gBET
Molecular Weight 277.64 g/mol
 
Component Elements PropertiesOriginal ValueComments
Indium, In 81.5 - 83.3 %
 82.7 %Theoretical
 
Descriptive Properties
Available Purity Level4N = 99.99%
 5N = 99.999%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Standard ITO Indium Tin Oxide
American Elements Indium Oxide Nanopowder
Indium Corp. IndiOx® In2O3 Type B Indium Oxide, Fine Powder
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
Indium Corp. Fine ITO Indium Tin Oxide

NNIN933 / 131572

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.