PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PP 1370 has an excellent balance of mechanical properties and is easy to injection mould. Typical applications include injection molded crates, boxes and tote bins for electronic components and other static sensitive devices (SSD). Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc. |