MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Easy disassembly.

Applications:

  • Ideal for thread locking small screws from loosening under vibration.
  • Ideal for fastening of ¼" (6mm) and smaller diameters.
  • Specifically suitable for applications such as adjustment of set screws and small diameter fasteners where easy disassembly is required.
  • Meets Military specifications: MIL-S-46163

Part Numbers for this data: 10-001, 10-010, 10-050, 10-250, 10-1000

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 923-26-2, 15625-89-5, 80-15-9 and 114-83-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Brookfield Viscosity 1000 cPRVT Spindle 3 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 3.00 - 10.0 MPaISO 10123; Compressive, Steel pins and collars
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hourHandling
 1.00 - 3.00 hourFunctional
 24.0 hourFull
Shelf Life 24.0 Month
 
Descriptive Properties
AppearancePurple
Chemical Resistance100% Initial Strength RetainedAcetone at 22°C, at 500hrs
 100% Initial Strength RetainedEthanol at 22°C, at 500hrs
 100% Initial Strength RetainedMotor Oil at 125°C, at 500hrs
 100% Initial Strength RetainedGasoline at 22°C, at 500hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 500hrs
 100% Initial Strength RetainedEthanol at 22°C, at 1000hrs
 100% Initial Strength RetainedMotor Oil at 125°C, at 1000hrs
 100% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 1000hrs
 80% Initial Strength RetainedAcetone at 22°C, at 1000hrs
 85% Initial Strength RetainedWater/Glycol at 87°C, at 1000hrs
 90% Initial Strength RetainedWater/Glycol at 87°C, at 500hrs
CompositionMethacrylate Ester
Max Screw Size1/4" / 6mm
Torque4 N.mPrevail, M10 steel nuts and bolts N.m, ISO 10964
 6 N.mBreakaway, M10 steel nuts and bolts N.m, ISO 10964
 9-21 N.mBreakloose, pre-torqued to 5 N.m, M10 steel nuts and bolts, ISO 10964
 9-21 N.mMax Prevail, pre-torqued to 5 N.m, M10 steel nuts and bolts N.m, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML040 / 135194

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.