MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ovako 7CrMoBS5 Imaform 5450 Steel, +QT
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Imaform is a high strength steel suitable for hot forging and direct hardening. It also can be hardened separately. Due to low carbon content the tempering is unnecessary. The structure in as hardened condition consist off lath martensite and/or bainite.

Information provided by Ovako

Key Words: 1.7278, 5CrB5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 250 - 330
@Thickness 30.0 - 60.0 mm
Round bar
 280 - 350
@Thickness <=30.0 mm
Round bar
Tensile Strength 800 - 1100 MPa
@Thickness 30.0 - 60.0 mm
Round bar
 900 - 1200 MPa
@Thickness <=30.0 mm
Round bar
Tensile Strength, Yield >= 700 MPa
@Thickness 30.0 - 60.0 mm
Round bar
 >= 750 MPa
@Thickness <=30.0 mm
Round bar
Elongation at Break 10 %
@Thickness <=30.0 mm
Round bar
 12 %
@Thickness 30.0 - 60.0 mm
Round bar
Reduction of Area 40 %
@Thickness <=30.0 mm
Round bar
 40 %
@Thickness 30.0 - 60.0 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 30.0 J
@Thickness <=30.0 mm,
Temperature 20.0 °C
Round bar
 40.0 J
@Thickness 30.0 - 60.0 mm,
Temperature 20.0 °C
Round bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 465 °CMS
 743 °CAC1
 833 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.0030 - 0.0050 %
Carbon, C 0.040 - 0.090 %
Chromium, Cr 1.2 - 1.5 %
Iron, Fe 96.6 - 97.76 %As Balance
Manganese, Mn 0.80 - 1.0 %
Molybdenum, Mo <= 0.15 %
Nickel, Ni <= 0.20 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S 0.050 - 0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NOVAKO367 / 234666

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.