MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Halsic RX (chemically doped) Silicon Carbide
Categories: Ceramic; Carbide

Material Notes: Exceptionally high-performance ceramics, offering absolute dimensional stability under high loads at elevated temperatures. Extremely high corrosion resistance. Very good thermal shock resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 - 3.10 g/ccFired
Porosity 0.10 - 5.0 %Apparent, water absorption
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 420 GPadynamic
 280 - 370 GPa
@Temperature 20.0 °C
Flexural Strength 80.0 - 400 MPa
@Temperature 20.0 °C
3-point
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.30 - 5.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 35.0 - 124 W/m-K
@Temperature 200 °C
Maximum Service Temperature, Air 1300 - 1650 °Cworking

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Nitride, Be3N2
CeramTec CD 101 Silicon Carbide, SiC-ZrB2
Morgan Advanced Ceramics Halsic I (reaction-bonded, silicon infiltrated) Silicon Carbide
Silicon Carbide, Alpha SiC
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC

CMORG56 / 90434

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.